IPC Validation Services - Qualified Products List (QPL) IPC-4101

IPC-4101: Specification for Base Materials for Rigid and Multilayer Printed Boards covers the requirements for base materials that are referred to as laminate or prepreg and listed in the specification sheets which are found after the main body of the standard. The specification sheets are to be used primarily for rigid and multilayer printed boards for electronic interconnections.

QPL (Qualified Products List) is used to qualify EMS suppliers’ products (including printed circuit boards) and the manufacturing sites where those products are produced. IPC-4101Companies on our Qualified Products List supply products that have been qualified to IPC standards.

The following companies have qualified their products for the IPC-4101 QPL
Arlon Electronic Materials, Rancho Cucamonga, CA, USA

Arlon Electronic Materials
9433 Hyssop Dr.
Rancho Cucamonga, CA 91730
Tel: 866-394-6508
Fax: 909-987-8541

IPC-4101 Qualified Base Materials QPL Listed Initial Certificate Date Listing Date Expiration Date
4101/40 33N 2/23/2018 3/25/2023 3/25/2028
4101/40 35N 2/23/2018 3/25/2023 3/25/2028
4101/40 85HP 5/20/2021 5/20/2021 5/20/2026
4101/40 85N 2/23/2018 3/25/2023 3/25/2028
4101/41 33N 2/23/2018 3/25/2023 3/25/2028
4101/41 35N 2/23/2018 3/25/2023 3/25/2028
4101/41 85HP 5/20/2021 5/20/2021 5/20/2026
4101/41 85N 2/23/2018 3/25/2023 3/25/2028
4101/42 37N 2/23/2018 3/25/2023 3/25/2028
4101/42 38N 2/23/2018 3/25/2023 3/25/2028
4101/43 84HP 5/19/2021 5/19/2021 5/19/2026
4101/43 85HP 5/11/2021 5/11/2021 5/11/2026
Laminate Supplier Audit   2/9/2018 3/1/2024 3/1/2027
Isola Laminate Systems (Suzhou) Co., Ltd.

Isola Laminate Systems (Suzhou) Co., Ltd.
121 Su Tong Road China
Singapore Suzhou Industrial Park Suzhou
Suzhou, Jiangsu, China 215021
Tel: 86-512-67610301

IPC-4101 Qualified Base Materials QPL Listed Initial Certificate Date Listing Date Expiration Date
IPC-4101/140 IS550H 5/14/2021 5/14/2021 5/14/2026
Laminate Supplier Audit   11/8/2021 11/8/2021 11/8/2024
Taiwan Union Technology Corp., Taiwan

Taiwan Union Technology Corp
803 Bo-ai Street
Zhubei City, Hsinchu County, Taiwan, 302045

Tel: +866 3 555 1103

IPC-4101 Certified Base Materials QPL Listed Initial Certificate Date Listing Date Expiration Date
IPC-4101/102 TU-933+ 4/18/2017 8/17/2022 8/17/2027
  TU-933 4/18/2017 8/16/2022 8/16/2027
  TU-933E 4/18/2017 8/16/2022 8/16/2027
  TU-933V 4/18/2017 8/16/2022 8/16/2027
  TU-943R 8/16/2022 8/16/2022 8/16/2027
  TU-943SN 8/16/2022 8/16/2022 8/16/2027
  TU-943SR 8/16/2022 8/16/2022 8/16/2027
  TU-943N 8/16/2022 8/16/2022 8/16/2027
IPC-4101/126 TU-872SLK 4/18/2017 8/4/2022 8/4/2027
  TU-768 4/18/2017 8/16/2022 8/16/2027
  TU-872LK 4/18/2017 8/16/2022 8/16/2027
  TU-872SLK SP 4/18/2017 8/16/2022 8/16/2027
IPC-4101/130 TU-862HF 4/18/2017 8/17/2022 8/17/2027
  TU-84P MF 4/18/2017 8/16/2022 8/16/2027
  TU-84P NF 4/18/2017 8/16/2022 8/16/2027
  TU-862T 4/18/2017 8/16/2022 8/16/2027
  TU-862S 4/18/2017 8/16/2022 8/16/2027
  TU-863 4/18/2017 8/16/2022 8/16/2027
  TU-863+ 4/18/2017 8/16/2022 8/16/2027
  TU-863NF 4/18/2017 8/16/2022 8/16/2027
  TU-865 4/18/2017 8/16/2022 8/16/2027
  TU-787LK 8/16/2022 8/16/2022 8/16/2027
  TU-900 8/16/2022 8/16/2022 8/16/2027
IPC-4101/134 TU-883 4/18/2017 8/17/2022 8/17/2027
  TU-883C 8/16/2022 8/16/2022 8/16/2027
  TU-883SP 8/16/2022 8/16/2022 8/16/2027
  TU-885 8/16/2022 8/16/2022 8/16/2027
  TU-885SP 8/16/2022 8/16/2022 8/16/2027
  TU-901 8/16/2022 8/16/2022 8/16/2027
  TU-883A 8/16/2022 8/16/2022 8/16/2027
Laminate Supplier Audit   2/6/2017 2/5/2023 2/5/2026
Ventec Electronics (Suzhou) Co., Ltd., P.R.C.

Ventec Electronics (Suzhou) Co., Ltd.
No. 308 Tai Shan Road, New District
Suzhou, Jiangsu Province 215009
P.R.C Tel: +86-512-68091810
Fax: 86-512-68099023

IPC-4101 Certified Base Materials QPL Listed Initial Certificate Date Listing Date Expiration Date
IPC-4101/40 VT-90HVT-901 10/27/2017 11/17/2022 11/17/2027
IPC-4101/41 VT-90HVT-901 10/27/2017 11/17/2022 11/17/2027
Laminate Supplier Audit   10/27/2017 2/28/2024 2/28/2027
IPC-4101/128 VT-441V 11/20/2019 11/20/2019 11/20/2024
IPC-4101/130 VT-447V 11/20/2019 11/20/2019 11/20/2024
IPC-4101/153 VT-441V 11/20/2019 11/20/2019 11/20/2024