Gold Brush Plating Rework of Power Logic Circuit Card Assembly in an Aerospace Electronic Application
Description
Selective electrodeposition (brush plating) was successfully used to rework a solder-contaminated, hard gold-plated copper flag connector for a circuit card assembly (CCA).